Microstructural Degradation of Superalloys during Service: Mechanical and/or Corrosion
A special issue of Crystals (ISSN 2073-4352). This special issue belongs to the section "Crystalline Metals and Alloys".
Deadline for manuscript submissions: closed (15 December 2021) | Viewed by 9473
Special Issue Editors
Interests: in situ; TEM; superalloy; microstructure; turbine blade
Special Issue Information
Dear Colleagues,
Superalloys used as blade material for gas turbines are strengthened by small intermetallic γ'-precipitates of the Ni3Al type. γ'-precipitation provides excellent mechanical properties at high temperatures, but its efficiency strongly depends on the size and morphology of the γ'-precipitates. During high temperature service in aircraft and power gas turbines, the γ/γ'-microstructure of nickel-base superalloys gradually degrades, i.e., coarsens and becomes rafted. This degradation of the microstructure deteriorates the mechanical properties. The relationship between microstructure and its properties are thus important to evaluate the service of the blade.
In this thematic issue, we invite contributions on the microstructure degradation of superalloys and the microstructural characterization and relationships between microstructure and its properties. The submitted works are expected to feature but are not limited to the following topics:
- Microstructural characterization of superalloys;
- Relationship between microstructural variation and its properties;
- Microstructural variation during corrosion of superalloys;
- Stress corrosion induced microstructural degradation in superalloys;
- Evaluation of serviced turbine blade;
- Newly developed superalloys: high entropy alloys, etc.
Prof. Dr. Yanhui Chen
Prof. Dr. Yunsong Zhao
Guest Editors
Manuscript Submission Information
Manuscripts should be submitted online at mdpi.longhoe.net by registering and logging in to this website. Once you are registered, click here to go to the submission form. Manuscripts can be submitted until the deadline. All submissions that pass pre-check are peer-reviewed. Accepted papers will be published continuously in the journal (as soon as accepted) and will be listed together on the special issue website. Research articles, review articles as well as short communications are invited. For planned papers, a title and short abstract (about 100 words) can be sent to the Editorial Office for announcement on this website.
Submitted manuscripts should not have been published previously, nor be under consideration for publication elsewhere (except conference proceedings papers). All manuscripts are thoroughly refereed through a single-blind peer-review process. A guide for authors and other relevant information for submission of manuscripts is available on the Instructions for Authors page. Crystals is an international peer-reviewed open access monthly journal published by MDPI.
Please visit the Instructions for Authors page before submitting a manuscript. The Article Processing Charge (APC) for publication in this open access journal is 2100 CHF (Swiss Francs). Submitted papers should be well formatted and use good English. Authors may use MDPI's English editing service prior to publication or during author revisions.
Keywords
- microstructure
- superalloys
- degradation
- creep
- oxidation